Alkaline activation of ceramic waste materials

RiuNet: Repositorio Institucional de la Universidad Politécnica de Valencia

Compartir/Enviar a

Citas

Estadísticas

  • Estadisticas de Uso

Alkaline activation of ceramic waste materials

Mostrar el registro sencillo del ítem

Ficheros en el ítem

dc.contributor.author Reig Cerdá, Lucía es_ES
dc.contributor.author Mitsuuchi Tashima, Mauro es_ES
dc.contributor.author Soriano, L. es_ES
dc.contributor.author Borrachero Rosado, María Victoria es_ES
dc.contributor.author Monzó Balbuena, José Mª es_ES
dc.contributor.author Paya Bernabeu, Jorge Juan es_ES
dc.date.accessioned 2015-04-17T15:07:41Z
dc.date.available 2015-04-17T15:07:41Z
dc.date.issued 2013-01
dc.identifier.issn 1877-2641
dc.identifier.uri http://hdl.handle.net/10251/48960
dc.description.abstract Ceramic materials represent around 45 % of construction and demolition waste, and originate not only from the building process, but also as rejected bricks and tiles from industry. Despite the fact that these wastes are mostly used as road sub-base or construction backfill materials, they can also be employed as supplementary cementitious materials, or even as raw material for alkali-activated binders This research aimed to investigate the properties and microstructure of alkali-activated cement pastes and mortars produced from ceramic waste materials of various origins. Sodium hydroxide and sodium silicate were used to prepare the activating solution. The compressive strength of the developed mortars ranged between 22 and 41 MPa after 7 days of curing at 65 C, depending on the sodium concentration in the solution and the water/binder ratio. These results demonstrate the possibility of using alkaliactivated ceramic materials in building applications. es_ES
dc.description.sponsorship The authors are grateful to the Spanish Ministry of Science and Innovation for supporting this study through Project GEOCEDEM BIA 2011-26947, and also to FEDER funding. They also thank Universitat Jaume I for supporting this research through Lucia Reig's granted research stay. en_EN
dc.language Inglés es_ES
dc.publisher Springer Verlag (Germany) es_ES
dc.relation.ispartof Waste and Biomass Valorization es_ES
dc.rights Reserva de todos los derechos es_ES
dc.subject Compressive strength es_ES
dc.subject Alkaline activation es_ES
dc.subject Waste management es_ES
dc.subject Ceramic waste es_ES
dc.subject.classification INGENIERIA DE LA CONSTRUCCION es_ES
dc.title Alkaline activation of ceramic waste materials es_ES
dc.type Artículo es_ES
dc.identifier.doi 10.1007/s12649-013-9197-z
dc.relation.projectID info:eu-repo/grantAgreement/MICINN//BIA2011-26947/ES/REUTILIZACION DE RESIDUOS CERAMICOS Y DE DEMOLICION EN LA PREPARACION DE NUEVOS MATERIALES GEOPOLIMERICOS/
dc.rights.accessRights Abierto es_ES
dc.contributor.affiliation Universitat Politècnica de València. Instituto de Ciencia y Tecnología del Hormigón - Institut de Ciència i Tecnologia del Formigó es_ES
dc.contributor.affiliation Universitat Politècnica de València. Departamento de Ingeniería de la Construcción y de Proyectos de Ingeniería Civil - Departament d'Enginyeria de la Construcció i de Projectes d'Enginyeria Civil es_ES
dc.description.bibliographicCitation Reig Cerdá, L.; Mitsuuchi Tashima, M.; Soriano, L.; Borrachero Rosado, MV.; Monzó Balbuena, JM.; Paya Bernabeu, JJ. (2013). Alkaline activation of ceramic waste materials. Waste and Biomass Valorization. 4:729-736. https://doi.org/10.1007/s12649-013-9197-z es_ES
dc.description.accrualMethod S es_ES
dc.relation.publisherversion http://dx.doi.org/10.1007/s12649-013-9197-z es_ES
dc.description.upvformatpinicio 729 es_ES
dc.description.upvformatpfin 736 es_ES
dc.type.version info:eu-repo/semantics/publishedVersion es_ES
dc.description.volume 4 es_ES
dc.relation.senia 258669
dc.contributor.funder European Regional Development Fund
dc.contributor.funder Ministerio de Ciencia e Innovación
dc.description.references Puertas, F., García-Díaz, I., Barba, A., Gazulla, M.F., Palacios, M., Gómez, M.P., Martínez-Ramírez, S.: Ceramic wastes as alternative raw materials for Portland cement clinker production. Cement Concrete Comp. 30(9), 798–805 (2008) es_ES
dc.description.references Ministerio de Fomento de España, Catálogo de Residuos Utilizables en Construcción (2010). http://www.cedexmateriales.vsf.es/view/catalogo.aspx . Retrieved on 6 Dec 2012 es_ES
dc.description.references Stock, D.: World production and consumption of ceramic tiles. Tile Today 73, 50–58 (2011) es_ES
dc.description.references Medina, C., Juan, A., Frías, M., Sánchez-de-Rojas, M.I., Morán, J.M., Guerra, M.I.: Characterization of concrete made with recycled aggregate from ceramic sanitary ware. Mater. Construcc. 61(304), 533–546 (2011) es_ES
dc.description.references Pacheco-Torgal, F., Jalali, S.: Reusing ceramic wastes in concrete. Constr. Build. Mater. 24(5), 832–838 (2010) es_ES
dc.description.references Lavat, A.E., Trezza, M.A., Poggi, M.: Characterization of ceramic roof tile wastes as pozzolanic admixture. Waste Manage. 29(5), 1666–1674 (2009) es_ES
dc.description.references Nuran, A., Mevlut, U.: The use of waste ceramic tile in cement production. Cement Concrete Res. 30, 497–499 (2000) es_ES
dc.description.references Pereira-de-Oliveira, L.A., Castro-Gomes, J.P., Santos, P.M.S.: The potential pozzolanic activity of glass and red-clay ceramic waste as cement mortars components. Constr. Build. Mater. 31, 197–203 (2012) es_ES
dc.description.references Van Deventer, J.S.J., Provis, J.L., Duxson, P., Brice, D.G.: Chemical research and climate change as drivers in the commercial adoption of alkali activated materials. Waste Biomass Valor. 1, 145–155 (2010) es_ES
dc.description.references van Deventer, J.S.J., Provis, J.L., Duxson, P., Lukey, G.C.: Reaction mechanisms in the geopolymeric conversion of inorganic waste to useful products. J. Hazard. Mater. A139, 506–513 (2007) es_ES
dc.description.references Duxson, P., Fernández-Jiménez, A., Provis, J.L., Lukey, G.C., Palomo, A., van Deventer, J.S.J.: Geopolymer technology: the current state of the art. J. Mater. Sci. 42(9), 2917–2993 (2007) es_ES
dc.description.references Bernal, S.A., Rodríguez, E.D., de Gutiérrez, R.M., Provis, J.L., Delvasto, S.: Activation of metakaolin/slag blends using alkaline solutions based on chemically modified silica fume and rice husk ash. Waste Biomass Valor. 3, 99–108 (2012) es_ES
dc.description.references Fernández-Jiménez, A., Palomo, A., Criado, M.: Microstructure development of alkali-activated fly ash cement: a descriptive model. Cement Concrete Res 35, 1204–1209 (2005) es_ES
dc.description.references Payá, J., Borrachero, M.V., Monzó, J., Soriano, L., Tashima, M.M.: A new geopolymeric binder from hydrated-carbonated cement. Mater. Lett. 74, 223–225 (2012) es_ES
dc.description.references Kourti, I., Amutha-Rani, D., Deegan, D., Boccaccini, A.R., Cheeseman, C.R.: Production of geopolymers using glass produced from DC plasma treatment of air pollution control (APC) residues. J. Hazard. Mater. 176, 704–709 (2010) es_ES
dc.description.references Puertas, F., Barba, A., Gazulla, M.F., Gómez, M.P., Palacios, M., Martínez-Ramírez, S.: Residuos cerámicos para su posible uso como materia prima en la fabricación de clínker de cemento Portland: caracterización y activación alcalina. Mater. Construcc. 56(281), 73–84 (2006) es_ES
dc.description.references Reig, L., Tashima, M.M., Borrachero, M.V., Monzó, J., Payá, J.: Nuevas matrices cementantes generadas por Activación Alcalina de residuos cerámicos. II Simposio Aprovechamiento de residuos agro-industriales como fuente sostenible de materiales de construcción, November 8–9, Valencia, Spain, pp. 199–207 (2010) es_ES
dc.description.references L. Reig, M.M. Tashima, M.V. Borrachero, J. Monzó, J. Payá: Residuos de ladrillos cerámicos en la producción de conglomerantes activados alcalinamente, I Pro-Africa Conference: Non-conventional Building Materials Based on Agroindustrial Wastes, October 18–19, Pirassununga, SP, Brazil, pp. 18–21 (2010) es_ES
dc.description.references García Ten F.J. Descomposición durante la cocción del carbonato cálcico contenido en el soporte crudo de los azulejos. Tesis de doctorado, Departamento de Ingeniería química, UJI (2005) es_ES
dc.description.references Baronio, G., Binda, L.: Study of the pozzolanicity of some bricks and clays. Constr. Build. Mater. 11(1), 41–46 (1997) es_ES
dc.description.references Zanelli, C., Raimondo, M., Guarini, G., Dondi, M.: The vitreous phase of porcelain stoneware: composition, evolution during sintering and physical properties. J. Non-Cryst. Solids 357, 3251–3260 (2011) es_ES
dc.description.references Carty, W.M., Senapati, U.: Porcelain-raw materials, processing, phase evolution, and mechanical behaviour. J. Am. Ceram. Soc. 81(1), 3–20 (1998) es_ES
dc.description.references ASCER, COACV, COPUT, ITC-AICE, WEBER ET BROUTIN – CEMARKSA: Guía Baldosa Guía de la baldosa cerámica. IVE: Conselleria d’Obres Públiques, Urbanisme i Transports, 4ª Ed. Valencia (2003) es_ES
dc.description.references Khater, H.M.: Effect of calcium on geopolimerization of aluminosilicate wastes. J. Mater. Civ. Eng. 24, 92–101 (2012) es_ES
dc.description.references Bondar, D., Lynsdale, C.J., Milestone, N.B., Hassani, N., Ramezanianpour, A.A.: Effect of adding mineral additives to alkali-activated natural pozzolan paste. Constr. Build. Mater. 25, 2906–2910 (2011) es_ES
dc.description.references Provis, J.L., Harrex, R.M., Bernal, A.S., Duxson, P., van Deventer, J.S.J.: Dilatometry of geopolymers as a means of selecting desirable fly ash sources. J. Non-Cryst. Solids 358, 1930–1937 (2012) es_ES
dc.description.references Duxson, P., Provis, J.L., Lukey, G.C., Mallicoat, S.W., Kriven, W.M., van Deventer, J.S.J.: Understanding the relationship between geopolymer composition, microstructure and mechanical properties. Colloid Surf. A 269, 47–58 (2005) es_ES
dc.description.references Tashima, M.M., Akasaki, J.L., Castaldelli, V.N., Soriano, L., Monzó, J., Payá, J., Borrachero, M.V.: New geopolymeric binder based on fluid catalytic cracking catalyst residue (FCC). Mater. Lett. 80, 50–52 (2012) es_ES
dc.description.references Komnitsas, K., Zaharaki, D., Perdikatsis, V.: Geopolymerisation of low calcium ferronickel slags. J. Mater. Sci. 42, 3073–3082 (2007) es_ES
dc.description.references Bernal, S.A., Gutierrez, R.M., Provis, J.L., Rose, V.: Effect of silicate modulus and metakaolin incorporation on the carbonation of alkali silicate-activated slags. Cement Concrete Res. 40, 898–907 (2010) es_ES
dc.description.references Tashima, M.M. Produccion y caracterizacion de materiales cementantes a partir del silicoaluminato calcico vitreo (VCAS). Tesis de doctorado, Departamento de Ingeniería de la construcción y de proyectos de ingeniería civil, UPV (2012) es_ES
dc.description.references Provis, J.L., van Deventer, J.S.J.: Geopolymerisation kinetics. 2. Reaction kinetic modelling. Chem. Eng. Sci. 62, 2318–2329 (2007) es_ES